Stretch Film Technical Data Sheet
This stretch film technical data sheet defines the structure, test conditions, and grade-specific evidence used to compare pallet wrap film. It covers hand, machine, pre-stretched, colored, and vented PE grades. Treat figures as typical or reference values unless an approved limit is stated. Confirm pre-stretch, puncture behavior, containment, unwind, and transport performance through representative sample testing before full use.
What This Dataset Covers
Use this dataset for comparison, inspection, approval, and trials. Link each result to type, thickness, batch, and method. It does not replace a roll specification or transport study. Shrink film, pressure-sensitive tape, and adhesive tests are outside this scope.
Review stretch film formats before testing.
Assess pre-stretched hand film separately because its supplied condition differs from conventional film.
From Resin System to Roll Geometry
Stretch film uses PE or LLDPE in mono- or multilayer construction. Cast and blown processing can change clarity, tear, puncture, cling, and unwind. Record process, layers, cling side, core, and winding condition.

Grade Approval Data
Item | Typical Value / Reference Range | Test Method or Condition | Notes |
Structure | Tested grade | Material record | Identify resin, process, layers, and type. |
Thickness | Grade value in um | Multi-position measurement | Read with tolerance and profile. |
Tensile / elongation | MD and TD values | Conditioned tensile test | State unit, width, speed, direction. |
Peel cling | Confirmed range | Film-to-film separation | State side, extension, temperature. |
Puncture / tear | Tested results | Separate methods | Do not combine failures. |
Recovery / retention | Stated extension | Extension-and-hold test | Supports retained-force comparison. |
Haze / transmittance | Grade-specific | Optical test | Only where visibility matters. |
Pre-stretch / containment | Project-confirmed | Wrapper and load trial | Depends on equipment and load. |
Publish values only when supported by a grade, batch test, specification, declaration, or project trial. Mark industry figures as references.
Evidence Behind Each Result
Test Item | What It Checks | Suggested Method or Reference | Why It Matters | When To Request It |
Thickness profile | Web variation | ISO 4593 or equivalent | Thin lanes reduce margin. | Downgauging or approval |
Tensile / elongation | MD and TD behavior | ASTM D882 or equivalent | Defines directional strength. | New grade or thickness |
Peel cling | Layer separation | ASTM D5458 or equivalent | Affects overlap and unwind. | Tail release or blocking |
Puncture | Probe resistance | ASTM D5748 or equivalent | Represents edge risk. | Sharp loads |
Recovery / retention | Retained stress | ASTM D5459 or equivalent | Relates to holding force. | Settling or storage |
Containment | Force after wrapping | Calibrated load trial | Connects film to load. | New load or wrapper |
A standard is a test basis, not certification. Record conditioning, direction, specimen size, speed, sample count, result rule, batch, and date.

Reading Performance Without Overreach
Thickness affects yield and puncture margin, but thicker film is not automatically better. Tensile strength is stress; force at break also reflects width and thickness. Elongation at break is a failure value, while recommended pre-stretch is equipment-confirmed. Peel cling is film-to-film interaction. Puncture and tear are different failures. Recovery and stress retention indicate retained holding force.
Compatibility Variables
Load weight, shape, surface, coating, edges, temperature, humidity, sunlight, storage, transport, equipment, operator method, film layers, and corner protection can change performance.
Controlled Trial Before Release
Record grade, batch, wrapper, pre-stretch, wrap force, pattern, load, and operator. Check roll edges, core shape, unwind, neck-down, breaks, tail retention, separation, puncture, movement, and barcode visibility. For a field-use checklist that connects these data points with real pallet movement, review how pallet wrapping methods affect load stability.
Recheck containment after 24 h, 72 h, and 7 days when relevant, then after handling.
Release only when criteria are met.

Where Data Drift Becomes Failure
Data Point | If Too Low | If Too High | Risk in Application | Check Before Full Use |
Thickness profile | Weak lanes | Excess material | Breaks or uneven corners | Map thickness |
Tensile strength | Early break | Poor conformity | Breaks or pressure points | Test MD and TD |
Elongation | Low extension | Weak recovery | Breakage or loose wrap | Compare recovery |
Peel cling | Tail release | Blocking | Loose tails or jerky unwind | Test at use temperature |
Puncture resistance | Easy penetration | Heavy construction | Holes and tear initiation | Wrap sharpest load |
Recovery / retention | Tension loss | Cargo compression | Shift or deformation | Measure after dwell |
Pre-stretch setting | Low yield | Neck-down or breaks | Unstable containment | Set operating window |
Preserving Roll Condition
Keep rolls dry and protected from sunlight, heat, pressure, contamination, and damage. Stabilize hot or cold rolls before testing. Recheck deformed material because storage can change cling, unwind, and repeatability.

Technical Routes Across the Site
Category, product, test, compatibility, and capability resources support this dataset without duplicating specifications.
Frequently Asked Technical Questions
How should a stretch film technical data sheet be read?
Confirm grade, thickness, direction, unit, method, conditioning, and data status. Compare equivalent results, then test the load and wrapper.
What is a typical value versus a guaranteed specification?
A typical value represents stated conditions. A guaranteed specification is an approved limit. Do not treat a reference value as a minimum.
Is recommended pre-stretch the same as elongation at break?
No. Elongation at break is a failure result. Recommended pre-stretch is confirmed with the film, equipment, and load.
Why can the same film perform differently?
Load shape, surface, edges, temperature, storage, wrap pattern, equipment, and operator method can change results. Sample testing is recommended.